Bio-compatible epoxy
2014-01-07
DEBASHIS MAJI
2014-01-07
André Bödecker
2014-01-07
Jan Thoren
2014-01-08
DEBASHIS MAJI
2014-01-08
DEBASHIS MAJI
2014-01-09
Jan Thoren
2014-01-09
James Guenes
2014-01-09
DEBASHIS MAJI
2014-01-10
André Bödecker
2014-01-09
Jan Thoren
2014-01-08
James Guenes
2014-01-08
王舒禹
Bio-compatible epoxy
André Bödecker
2014-01-10
Hi all,

that's correct. You can call PDMS also silicone (not silicon!).
Regards,
André

-----Ursprüngliche Nachricht-----
Von: [email protected]
[mailto:[email protected]] Im
Auftrag von DEBASHIS MAJI
Gesendet: Donnerstag, 9. Januar 2014 18:38
An: General MEMS discussion
Betreff: Re: [mems-talk] Bio-compatible epoxy

Dear Jan,
PDMS stands for Polydimethlysloxane. It is a polymer often used for making
biomedical devices. I need the epoxy to fix my device (made of PDMS) over
some
PE (polyethylene)  or PU (polyurethane) substrates.
Thanks for your help anyways.


On Thu, Jan 9, 2014 at 2:43 AM, Jan Thoren  wrote:

> Our binder is very fast drying- like 5-10 minutes- I have a background in
> architecture and do not know what PDMS is --
> so please describe it or let me know what the letters stand for. thanks-
> Jan
>
>
>
>
> Recreating Architecture through Nanotechnology
>
>
> JanThoren-president
> NanoArchitech
> Architectural Technology Group
> San Francisco Bay Area
>
> 707 741-7919 direct line
>
> nanoarchitech.com
>
>
>
>
>
>
>
> On Wed, Jan 8, 2014 at 8:52 AM, DEBASHIS MAJI  >wrote:
>
> > Thanks all for your help... I shall try out the links and search for the
> > epoxy.
> > I tried fixing with PDMS, but my substrate itself is PDMS and it takes
> some
> > time to cure. so i am looking for an adhesive that binds quicker.
> > I shall try out the links and search for the epoxy.
> >
> >
> >
> > On Wed, Jan 8, 2014 at 10:01 PM, DEBASHIS MAJI  > >wrote:
> >
> > > Thanks Jan,
> > > My material is PDMS. I would like to fix it on some PE or PU
> substrates.
> > > Would it be suitable for fixing of PDMS materials?
> > >
> > >
> > > On Tue, Jan 7, 2014 at 8:50 PM, Jan Thoren  wrote:
> > >
> > >> I have a material which is friendly to the human body and has very
> good
> > >> bonding abilities . It is non - conductive.
> > >> What is the substrate material?
> > >> I would be willing to test it if you can provide a sample of the
> > material.
> > >> My email is [email protected]
> > >>
> > >>
> > >>
> > >>
> > >> Recreating Architecture through Nanotechnology
> > >>
> > >>
> > >> JanThoren-president
> > >> NanoArchitech
> > >> Architectural Technology Group
> > >> San Francisco Bay Area
> > >>
> > >> 707 741-7919 direct line
> > >>
> > >> nanoarchitech.com
> > >>
> > >>
> > >>
> > >>
> > >>
> > >>
> > >>
> > >> On Sun, Jan 5, 2014 at 10:27 PM, DEBASHIS MAJI <
> [email protected]
> > >> >wrote:
> > >>
> > >> > Dear All,
> > >> >
> > >> > I am searching for a some biocompatible epoxy (not conductive
epoxy)
> > to
> > >> fix
> > >> > my sensor over a substrate for some in vitro animal experiments.
can
> > >> > anybody kindly provide me names of few such epoxies?
> > >> >
> > >> > Thanks in advance.
> > >> >
> > >> > --
> > >> > Thanks & Regards
> > >> >
> > >> > Debashis Maji,
> > >> > Senior Research Fellow,
> > >> > PhD Scholar - School of Medical Science & Technology,
> > >> > IIT Kharagpur, India - 721302
> > >> > _______________________________________________
> > >> > Hosted by the MEMS and Nanotechnology Exchange, the country's
> leading
> > >> > provider of MEMS and Nanotechnology design and fabrication
services.
> > >> > Visit us at http://www.mems-exchange.org
> > >> >
> > >> > Want to advertise to this community?  See http://www.memsnet.org
> > >> >
> > >> > To unsubscribe:
> > >> > http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > >> >
> > >> _______________________________________________
> > >> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> > >> provider of MEMS and Nanotechnology design and fabrication services.
> > >> Visit us at http://www.mems-exchange.org
> > >>
> > >> Want to advertise to this community?  See http://www.memsnet.org
> > >>
> > >> To unsubscribe:
> > >> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > >>
> > >
> > >
> > >
> > > --
> > > Thanks & Regards
> > >
> > > Debashis Maji,
> > > Senior Research Fellow,
> > > PhD Scholar - School of Medical Science & Technology,
> > > IIT Kharagpur, India - 721302
> > >
> >
> >
> >
> > --
> > Thanks & Regards
> >
> > Debashis Maji,
> > Senior Research Fellow,
> > PhD Scholar - School of Medical Science & Technology,
> > IIT Kharagpur, India - 721302
> > _______________________________________________
> > Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> > provider of MEMS and Nanotechnology design and fabrication services.
> > Visit us at http://www.mems-exchange.org
> >
> > Want to advertise to this community?  See http://www.memsnet.org
> >
> > To unsubscribe:
> > http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> >
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>



--
Thanks & Regards

Debashis Maji,
Senior Research Fellow,
PhD Scholar - School of Medical Science & Technology,
IIT Kharagpur, India - 721302
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation