MEMSnet Home: MEMS-Talk: RE: Diamond CVD
RE: Diamond CVD
1999-07-07
Karl Cazzini
RE: Diamond CVD
Karl Cazzini
1999-07-07
One of the best companies in the business of CVD diamond films is Norton
Diamond Film, Northboro Massachusetts.

******************************
* Karl H. Cazzini (Ph.D)     *
* Conifer Group & Associates *
* 116 Cochituate Road        *
* Framingham MA 01701        *
* USA                        *
*                            *
* Tel(W): (508) 620 8845     *
* Fax(W): (508) 620 8839     *
* Tel(H): (508) 875 2009     *
******************************

-----Original Message-----
From: [email protected] [mailto:[email protected]]On Behalf Of Sandeep
Vohra
Sent: Tuesday, July 06, 1999 12:28 PM
To: [email protected]
Subject: Diamond CVD



Looking for company(s) to do DIAMOND CVD work.  Hoping to get layer
thicknesses of 50 to 75 microns.  High thermal conductivity and electrical
resistivity desired.


Please send respnses to : [email protected]


thank you


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation