MEMSnet Home: MEMS-Talk: Re: Diamond CVD
Re: Diamond CVD
1999-07-07
MARIO ROBLES
Re: Diamond CVD
MARIO ROBLES
1999-07-07
Helo Sandeep,

I may be able to help. I work for Tanaka Systems and we represent Asahi
Diamond of Japan.  We sell their dicing blades, grinding wheels, ID
blades, CMP conditioners and other diamond tooling. These are normally
sold to semiconductor or medical companies.

If you can tell me what the application is and some more specific
requirments I will check with Asahi to see if we can supply what you are
looking for.

Please respond to this address [email protected]

Thank you!

Mario Robles
650-966-8001 ph
650-966-1881 fax


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review