Adhesive for Optics Fiber and Silicon chip
Andrew Sarangan
2014-10-27
Instead of bringing the chip to the fiber, fix the fiber in a standard
fiber mount and move with a xyz translation stage to contact the chip, just
like you would for optical coupling.
On Oct 27, 2014 10:49 AM, "DEEPAN KISHORE KUMAR" 
wrote:

> Hi All,
>
> We are trying to bond a small silicon chip at the edge of the 150 micron
> optical fiber, we are trying to bring the chip in contact with the fiber,
> but the micro-manipulator is not sufficient as we tend to break the fiber
> very easily.  Any ideas about what adhesive and what technique can be used
> for bonding a chip on the tip of a fiber ?
>
> Thanks,
> Deepan
>
>
>
>
> --
> Sent from iPhone, please excuse brevity.
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing