Hello,

We are using shadow contact masks made of Si for one of the
metalization processes. They are fabricated by cutting holes wih
laser in thin silicon wafers, so they can be very easily damaged
during the alignment procedure. The alternative substrate for mask
fabrication would be metal but the problem is the flatness of the
mask after fabrication because we need around 100 holes on 100 mm
wafer.

Does anyone have experience with shadow masks and/or know the
supplier of shadow masks made of metal?

Wlodek Kaplan

*


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMStaff Inc.
University Wafer