MEMSnet Home: MEMS-Talk: Negative photoresist
Negative photoresist
1999-09-07
SILLON Nicolas
Negative photoresist
SILLON Nicolas
1999-09-07
Hello,
I'm looking for a high resolution negative (or reversible) photoresist for
gold electroplating. I tried AZ 5214 but it doesn't seem to be compatible
with gold plating.
Any advice  is appreciated.
Thank You.

SILLON Nicolas
CEA / Leti
DMITEC / SIA / ES
17 rue des Martyrs
38 054 GRENOBLE Cedex 9
Tel:   (33) 4 76 88 36 01
Fax:  (33) 4 76 88 94 56


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing