MEMSnet Home: MEMS-Talk: Re: Thermal mismatch Pyrex/Al2O3
Re: Thermal mismatch Pyrex/Al2O3
1999-12-04
Steve Creswick
Re: Thermal mismatch Pyrex/Al2O3
Steve Creswick
1999-12-04
You wrote

>Hi,
I'm trying to solve a thermal-mismatch problem between two parts,
consisting of Pyrex glass and aluminium-ceramik(al2o3) by bonding them
with an elastic adhesive.
Could someone give me hints on which adhesive would be suitable?
Thank you in advance.

Sincerly, W.Brueck



Regarding your posting,

It would be very helpful to detail the environmental conditions (peak
temperature, operating temp, times, chemical exposures, etc) you wish the
assembly to endure.

Any strength requirements?

Any particular outgassing constraints?

The size of your assembly would also be of value.


Silicones (RTV or heat cure) or acrylics are the first to come to mind



Steven Creswick - CTS Microelectronics
 Mgr. Advanced Process Development
              1201 Cumberland Avenue
                  W. Lafayette, IN  47906

       E-Mail  [email protected]
                      PH  765 463 2565 - main
                      PH  765 497 5303 - direct
                      FX   765 497 5399


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
University Wafer