MEMSnet Home: MEMS-Talk: Re: Micromachined heaters and heat exchangers
Re: Micromachined heaters and heat exchangers
1999-01-06
[email protected]
1999-01-06
[email protected]
1999-01-07
CJ Kim
1999-01-11
[email protected]
1999-01-18
Stephen Greer
Re: Micromachined heaters and heat exchangers
CJ Kim
1999-01-07
 $)C You may want to see the MS thesis of my student (on chip cooling
with microchannels). He can be contacted at  Tim Yeh . He
made heaters and T sensors on chip.

Perry Skeath wrote:

> Hello, MEMS-list subscribers -
>
> We are interested in heating a liquid as it passes through a chip.  Does
> anyone have literature references on either of the two following subjects
> that they would be willing to share:
>
> 1.  Chip-heater resistors
>
> 2.  Micromachined heat exchangers
>
> Thank you in advance for your help!
>
> Perry Skeath
> SprayChip Systems Corp.
> 9841 Greenbelt Road, Suite 101
> Seabrook MD 20706-6270
> (301) 552-5570 voice
> (301) 552-5573 fax
>

   --  $)C =================================================
Chang-Jin "CJ" Kim, Ph.D.
Associate Professor
Mechanical and Aerospace Engineering Department
38-137 Engineering IV. Bldg.
University of California, Los Angeles (UCLA)
Los Angeles, CA 90095-1597
Telephone: (310) 825-0267   FAX: (310) 310-206-2302
E-mail: [email protected]   Internet: http://cjmems.seas.ucla.edu
=================================================


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.