I would suggest speaking with Loctite and 3M about their adhesives.  You can
find their phone numbers in the Thomas Registry

Tina

> ----------
> From:         Aiping Zheng
> Reply To:     Aiping Zheng;[email protected]
> Sent:         Friday, December 11, 1998 11:42 AM
> To:   [email protected]
> Subject:      looking for adhesive
>
> This is a multi-part message in MIME format.
>
> ------=_NextPart_000_0007_01BE24EA.82638520
> Content-Type: text/plain;
>       charset="iso-8859-1"
> Content-Transfer-Encoding: quoted-printable
>
> Dear Colleague,
>
> I am a graduate student in Louisiana Tech University majored in chemical =
> engineering. My project is microreactor where cyclohexane dehydrogenate =
> to produce benzene. The reaction is supposed to happen at 250C. I have =
> problem to find adhesive which could operate at 300C. The adhesive is =
> used to binding metal.
>
> Thank you for any suggestion and idea.
>
>
> Aiping Zheng
>
>
>
>
> ------=_NextPart_000_0007_01BE24EA.82638520
> Content-Type: text/html;
>       charset="iso-8859-1"
> Content-Transfer-Encoding: quoted-printable
>
> 
> 
> 
>
>  http-equiv=3DContent-Type>
> 
> 
> 
> 
Dear Colleague,
>
 
>
I am a graduate student in color=3D#000000>Louisiana=20 > Tech University majored in chemical engineering. My project is=20 > microreactor where cyclohexane dehydrogenate to produce benzene. The = > reaction is=20 > supposed to happen at 250C. I have problem to find adhesive which could = > operate=20 > at 300C. The adhesive is used to binding metal.
>
 
>
Thank you for any color=3D#000000>suggestion=20 > and idea.
>
 
>
 
>
Aiping Zheng
>

 
>
 
> > ------=_NextPart_000_0007_01BE24EA.82638520-- > > >
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics