MEMSnet Home: MEMS-Talk: AW: SI mechanical properties
AW: SI mechanical properties
1999-02-08
[email protected]
AW: SI mechanical properties
[email protected]
1999-02-08
Hi,

maybe you can find further information in:

'Materials Handbook für Hybrid Microelectronics'
J.A. King, Teledyne Microelectronics, Los Angeles, California
1988, ISBN 0-89006-325-7

ARTECH HOUSE INC.
685 Canton Street
Norwood, MA 02062

Hope it will help,
Timm

**************************************************
* Timm Leuerer                                   *
* Institut fuer Werkstoffe der Elektrotechnik    *
* Sommerfeldstr. 24                              *
* RWTH-Aachen                                *
* 52056 Aachen                              *
* Germany                                        *
* Tel: ++49 / (0)241 / 80-7836                   *
* Fax: ++49 / (0)241 / 8888-392                  *
* [email protected]                     *
**************************************************


> -----Ursprüngliche Nachricht-----
> Von:  Fadi Ben Achour [SMTP:[email protected]]
> Gesendet am:  Mittwoch, 3. Februar 1999 18:55
> An:   [email protected]
> Betreff:      SI mechanical properties
>
> Hello
> I am a graduate student at University of Minnesota and I am looking from
> mechanical properties of Silicon. More specifically i want the value of
> the stress at which silicon would fail in , compresion and tension. If you
> can kindly send this information with a refrence it will be greatly
> appreciated.
>
> Fadi Ben Achour
>
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Addison Engineering