Hi,

Thanks a lot for all respons I've got to solve my problem. Here comes
a list of companies you can try to fabricate shadow masks:

American Etching and Anufacturing
fax +1 818 896 0095
http://www.aem.com/products.htm

Industrial Engraving Company, Inc.
fax +1 610 253 0550
http://www.indengco.com/

Micro Prats, Inc.
fax +1 651 452 1926

Micro-Chem Inc.
fax +1 408 970 9380

Photo Stencil Inc.
fax +1 719 599 4334
http://www.photostencil.com/

Photo-Chem Etch Corporation
fax +1 818 767 3547
http://www.photo-chem.com/

Qualitetch Components Ltd.
fax +44 1354 650385
http://www.qualitetch.co.uk/

Vacco Industries
fax +1 626 350 0533
http://www.vacco.thomasregister.com/olc/vacco/home.htm


Regards,

Wlodek Kaplan
*


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.