Yit-shun Leung Ki
Re: Glass Etch
Peter C. Simpson
1999-03-03
Anisotropic glass etching is difficult if you want to go deeper than a
micron.  I worked at Cornell several years ago on isotropic glass etching
with Prof. Harold Craighead.  He has also worked on some anisotropic etching
and may be a good resource.

Regards,

Peter

At 09:08 PM 3/1/99 -0500, you wrote:
>Hi,
>
>I wonder if I could get some advice from you. Does anybody has done
>something on glass (e.g. Pyrex or Corning #7740) etching
>anisotropically?
>
>Thanks a lot!
>
>Jean.
>
>
>
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation