Re: How does everybody cut the glass? (7740)
1999-03-23
Wen H. Ko
1999-03-24
Lee Jia-Hong
1999-03-24
Bill Stockdale/John Baker
Re: How does everybody cut the glass? (7740)
Bill Stockdale/John Baker
1999-03-24
Jerry -

Our firm provides glass wafer substrates without holes for MEMS silicon to
glass and glass to glass bonding.  You can order in a variety of sizes.  See
our website at www.sensorprepservices.com.  Please contact me if we can help
you.

Thank you,

Kris Burgeson
Sensor Prep Services
-----Original Message-----
From: Lee Jia-Hong 
To: [email protected] 
Date: Tuesday, March 23, 1999 12:07 PM
Subject: How does everybody cut the glass? (7740)


>Hi, everybody:
>    I am micromachining on 7740 glass, but I have problem to cut my 7740
>glass into pieces, in order not to waste when experiments...
>    Does anybody have good comments for me? or some experience to share...
>thanks!
>Best regards,
>____________________________________________
>Jerry Lee
>(Jia-Hong Lee)
>Insitute of Applied Mechanics,
>National Taiwan University
>Taipei, Taiwan, ROC
>e-mail:
>[email protected]
>[email protected]
>"Try then error is better than no try"
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation