MEMSnet Home: MEMS-Talk: Re: TMAH resistant wax
Re: TMAH resistant wax
1999-04-12
Steve G Forgrieve
1999-04-12
Amit Shiwalkar
Re: TMAH resistant wax
Steve G Forgrieve
1999-04-12
Why do you want to use wax? I am assuming the side of the wafer you
want to etch will be patterned somehow, perhaps using silicon nitride.
When you grow the silicon nitride it will grow on both sides of the wafer
anyway. Grow a layer of photoresist on both sides. When you expose and
develop one side of the wafer the other side will remain protected.
 On Wed, 7 Apr 1999, Shivalik Bakshi wrote:

> Dear MEMS Researchers,
>
> Would you know of a wax material that I can use to protect one side of a wafer
while etching the other side in TMAH (or EDP)?
>
> Thanks,
> Shivalik
>
> ----------------
> Shivalik Bakshi,
> School of Engineering Science,
> Simon Fraser University,
> Burnaby, BC V5A 1S6
> Canada
>
> Email: [email protected]
> Tel: (604) 298-6847
>
>
>
>
>

Steve Forgrieve
Department of Electrical Engineering
The University of Edinburgh
King's Buildings
Mayfield Rd
Edinburgh EH9 3JL
(Int +44) 131 650 5665 (enquiries)
email: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering