MEMSnet Home: MEMS-Talk: Re: how to measure the depths of muli-layers
Re: how to measure the depths of muli-layers
1999-04-19
Jaideep Mavoori
1999-04-19
Jaideep Mavoori
1999-04-19
Justin Mansell
1999-04-21
Rajeshuni Ramesham
Re: how to measure the depths of muli-layers
Justin Mansell
1999-04-19
>i wanna know the depth of layers.
>i have 4 multi layer(silicon dioxide, silicon nitride, poly-silicon,
>silicon nitride) wafer. but i don't know the way to measure the depth
>of each layer during etching.
>but i can't make a step.
>because right now i can't use dry etch.
>so i wanna use an ellipsometer.
>if you have info about it let me know.
>thanks in advance.

I use an ellipsometer made by a company called Sopra (www.sopra-sa.com).
They are very helpful.  Try contacting them and see if they will measure
your sample for you.

Justin Mansell  |       "Only a risk tests the reality of a belief"
Ginzton Laboratory      |                       - C. S. Lewis
445 Via Palou St.       |
Stanford, CA 94305      |


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review
University Wafer