Re: dry etch Pt
Jayant Neogi
1999-04-21
Hi:

We have been using Iodine gas to etch into Pt and it works great.

Jayant
*************************************************
Jayant Neogi
Vice President & Chief Technical Officer
Norsam Technologies Inc.
Ph# (503) 640-0586
Fax  (503) 640-8117
http://www.norsam.com
*************************************************
-----Original Message-----
From: Emmanuel Dubois 
To: [email protected] 
Date: Wednesday, April 21, 1999 11:27 AM
Subject: dry etch Pt


>
>Does anybody know which gas is suitable for dry etching platinum ?
>
>Thanks
>
>Emmanuel Dubois
>
> ___________________________________________________________________
>          __  ____  __       __  __  __
>       / /_/ / / / / /  _ / /_  /_/ / /
>      / /_  / / / / /    / __/ /_  / /
>
>     Institut d'Electronique et de
>     Microelectronique du Nord
>     UMR CNRS 8520
>     Departement ISEN
>     Avenue Poincare B.P.69
>     59652 VILLENEUVE D'ASCQ  CEDEX
>     tel: (+33) 3 20 19 79 16
>     fax: (+33) 3 20 19 78 84
>     e-mail:[email protected]
>     http://www.isen.fr/isen-lci/quest
>
>___________________________________________________________________
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.