hi people,

i'll be very glad if someone could tell me the stress ultimate failure under
bending of silicon (100). Thanx !


Sinan HALIYO

Laboratoire de Robotique de Paris
10-12 av. de l'Europe 78140 Velizy - FRANCE

tel : (33) 1 39.25.49.74
fax : (33) 1 39.25.49.67
mail: [email protected]