Patterning of silicon nitride using KMER resist
1999-05-07
vikas Galhotra
Patterning of silicon nitride using KMER resist
vikas Galhotra
1999-05-07
Hello Colleagues:

I am looking for a photoresist to pattern silicon nitride thin film.
Specifically I wanted to use KMER resist as it goes well with dilute
NaOH solution which I am planning to use as an etchant for silicon
nitride. If someone can give me some information where to get this KMER
resist from, I will appreciate that very much.

Alternatively If someone can suggest
(1) some other photoresist that goes well with dilute solution of NaOH
or
(2) some other etchant for silicon nitride (other then anything that
contains HF)

I will be very thankful.

My e-mail address is "[email protected]"

Thanks in advance

Vikas Galhotra

Research Scientist
TiNi Alloy Company


_________________________________________________________
Do You Yahoo!?
Get your free @yahoo.com address at http://mail.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics