Re: Electroless Gold Plating
2000-06-12
ARGONIDE
2000-08-13
Argonide Nanomaterials Group
Re: Electroless Gold Plating
ARGONIDE
2000-06-12
Glenn & Group,
We are working on a process for applying a electroless mixture onto an
activated surface at room temperature to metallize the substrate.  We have
used painting and other means of application including silk screening would
be practical.  The process is electroless and works for copper and silver
and we have done a few tests with gold.  The substrate would have to be
sensitized as in conventional electroless.  We also provide nanosize metal
powders that can be incorporated into such mixtures.  For further info
drop an e-mail.

Cindi Prorok
Argonoide Nanometals Group
www.argonide.com

Glen Smith wrote:

> Hi there,
>
> Looking for vendors that will do gold electroless
> plating for 6" wafers.  Or any vendor that will
> sell the equipment or supplies for it?
>
> Thanks
>
> glen
> ________________________________________________________________________
> Get Your Private, Free E-mail from MSN Hotmail at http://www.hotmail.com
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMStaff Inc.
MEMS Technology Review