A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: Flat Silicon Wafers
Re: Flat Silicon Wafers
2000-09-13
Kenneth Smith
Re: Flat Silicon Wafers
Kenneth Smith
2000-09-13
if your looking for polished surfaces (front and back), the best flatness that I
have seen is from Ultrasil Corporation in Hayward where they can supply 4"
wafers
at  0.6-0.9 um  TTV and <1 um on 150mm wafers with Double Side Polishing.

Dont know of anything better- Should you find some , let me know as well.

Ken

Justin Mansell wrote:

> Can someone recommend a silicon wafer vendor for very flat wafers?  I'm
> looking ideally for less than a wave at 633nm over the entire wafer.
> Justin Mansell          |       "Only a risk tests the reality of a belief"
> Ginzton Laboratory      |                       - C. S. Lewis
> 445 Via Palou St.       |
> Stanford, CA 94305      |       (650) 723-2666 (fax)    (650) 725-2284
(office)
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
MEMStaff Inc.