1996-04-12
Jean-Francois MAINGUET (@SEG)
SOI wafers
Jean-Francois MAINGUET (@SEG)
1996-04-12
Michel,

The company below produces SOI wafers:


SOITEC sa
15 rue des Martyrs
38054 GRENOBLE cedex 9
FRANCE
phone: +33 76 88 38 76
fax: +33 76 88 54 85
regards,

Jean-Francois Mainguet
[email protected]
------------------- your message:
Greetings All !

        I'm a poor Aussie stuck down under... I need some assistance in locating
one or more companies to which I can place an order for some (Okay 10 - 20)
Silicon On Insulator Wafers.. The only catch is the top layer of Si has to be in
the vacinity of 10 - 15 micron thick.  So this definately falls into the custom
chip range..

        Any assistance would be greatly appreciated.

        Thanks,

                Michel A. Rosa.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing