MEMSnet Home: MEMS-Talk: Au and Ni together
Au and Ni together
2000-11-07
Yahong Yao
Au and Ni together
Yahong Yao
2000-11-07
Dear Colleague,

Au/Cr pattern is formed on top of SiO2 (1um thick) by liftoff process. But I
have to etch SiO2 to get the same pattern as Au. I know Au is not a good
mask for RIE, so I want to put Ni on top of Au so that a Ni/Au/Cr stack will
be the RIE mask. Q: Can Au and Ni be put together? I know Al and Au can not
be put together. Any suggestion is highly appreciated.

Yahong


_________________________________________________________________________
Get Your Private, Free E-mail from MSN Hotmail at http://www.hotmail.com.

Share information about yourself, create your own public profile at
http://profiles.msn.com.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group