Hello,

Virginia Semiconductor Inc can offer you thin silicon bonded to thick silicon/
SiO2. Contact VSI at (540) 373-2900.

Stephen Jones

>>
>> Dear "Poor Aussie":
>>
>> Since you need SOI with a thick layer (15 micron) of
>> silicon film, you may only have the option of Bonded-
>> and-Etchback SOI (BESOI) which permits such thicker
>> layers.  The alternative is (oxygen-implanted) SIMOX
>> wafers that subsequently require epi-silicon grown
>> on a thin 200-nm silicon film.
>>
>> For BESOI, you might try contacting either SiBond
>> L.L.C. (Hopewell Junction, NY) or Shin-Etsu Handotai -
>> SEH (Isobe, Japan or Washington State, USA).
>>
>> ----R.W. Griffith
>>
>>
>>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Addison Engineering
University Wafer