Cleaning up metal flakes after liftoff
2001-05-29
Dwarakanath Geerpuram
Cleaning up metal flakes after liftoff
Dwarakanath Geerpuram
2001-05-29
hi
I am trying to do a liftoff step for Cobalt.The liftoff is coming out ok but
some metal flakes coming off the wafer are sticking on to my pattern.how can I
remove them?

Thanks
Dwarakanath

"Beware of entrance to a quarrel; but being in,
Bear't that the opposed may beware of thee."
                         -Polonius to Laertes
                          From "Hamlet" , William Shakespeare


Dwarakanath Geerpuram
1028, S.May St. #1F
Chicago, IL 60607

Ph:  (312)316 1091(M)
     (312)413 7581(W)
http://www.eecs.uic.edu/~dgeerpur


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics