MEMSnet Home: MEMS-Talk: chromium evaporation
chromium evaporation
2001-02-14
[email protected]
chromium evaporation
[email protected]
2001-02-14
I want to deposit chromium using e-beam evaporation. But I discovered it is
not simple. It seems like chromium vaporizes even before it melts. Could
anybody give me any suggestion? Is it possible to deposit chromium use
ebeam?

Thanks!

Jessie Zhang, PhD
Thin Film Engineer
Paratek Microwave, Inc.
[email protected]