MEMSnet Home: MEMS-Talk: BOE undercutting of poly beams
BOE undercutting of poly beams
2001-08-03
E.McCloud
2001-08-03
E.McCloud
2001-08-06
E.McCloud
BOE undercutting of poly beams
E.McCloud
2001-08-06
Thanks to all the advice, and information given.  I'll be spending most of my
time doing further research and phone calls to see what I can take as a good
next step.  I'll also make sure to keep you updated as to my progress, and
hopeful success.

-Eddie
reply