Gokhan Percin
2001-08-14
Dear Thai,

Please check G.S. Kino and B. A. Auld's books. They have appendices giving
the properties of different piezoelectrics including ZnO.

Regards,

GP.

G. S. Kino,
Acoustic Waves: Devices, Imaging, and Analog Signal Processing,
Prentice-Hall, Inc., Englewood Cliffs, New Jersey,

B. A. Auld,
Acoustic Fields and Waves in Solids, 2nd ed., vol. 1,
Robert E. Krieger Publishing Company, Malabar, Florida,


On Tue, 14 Aug 2001, Thai Nguyen wrote:

>
>
> Hi,
>
>  I would like to know the properties of Aluminum Nitride and Zinc Oxide
> (curie temp).  I would be very grateful if anyone could
> help me. Thanks,
>
> Thai Nguyen
>
>
>
> Please visit our website at http://www.dbrgroup.com
> This email and any files transmitted with it are confidential
> and are intended solely for the use of the individual or
> entity to whom they are addressed.
>
> _______________________________________________
> mems-talk mailing list
> [email protected]
> http://fab.mems-exchange.org/mailman/listinfo/mems-talk
>

------------------------------------------------------------------
Homepage:          http://www.stanford.edu/~percin
E-mail  :          [email protected]
                   [email protected]
Address : (Home)   316 Quinnhill Ave
                   Los Altos, CA 94024
Phone   : (Home)   (650) 947-9487
                   (650) 248-6584
------------------------------------------------------------------



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing