Hello, I am wondering if anyone has any experience in bonding glass of
different thickness.  We are trying to bond one piece of glass (~1.8 mm
thick) to another piece of glass (~100 um thick) but are having trouble
with bubbles forming.  Any advice would be appreciated.  Thanks.

Mike