Adnan Merhaba
gold electroplating
Adnan Merhaba
2001-09-26
Hello,

My name is Adnan Merhaba and I am a process engineer with the American
technical ceramics. I have a question regarding pattern plating of gold, we
are currently using a cyanide bath and use 1818 photoresist to mask the
areas not to be plated, however during the plating process, we often find
that the resist shrinks, and hence plating occurs in region where it is not
supposed to. Does anyone know the root cause of this and what are the
possible solutions to avoid it?

Thank you
Regards,
Adnan



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review
University Wafer