Hello!
I am facing problem in etching Ni-Ti-Cu alloys for optical microscopy. The
normal etchant for Ni-Ti alloys does not work. Can you please suggest me some
etchants for Ni-Ti-Cu alloys?

kind regards
S.K.Bhaumik