Surface Energy
2001-10-01
Andrew F Rutkiewic
2001-10-02
[email protected]
Surface Energy
Andrew F Rutkiewic
2001-10-01
Dr. Luginbuhl;

I suggest that you characterize the specific surfaces you are working with by
measuring their surface energy by measuring the contact angle of various
liquids by the methods of Zisman etal as mentioned in the attached web site.

Regards;
Andrew F Rutkiewic VP
TRACE Photonics, Inc
Tijeras, NM