How to make a TiO2 film W/O CVD?
2001-10-09
Ralph Jin(季寶琪)
2001-10-10
Stefan Wiechmann
How to make a TiO2 film W/O CVD?
Ralph Jin(季寶琪)
2001-10-09
Dear All:

Can someone give some suggestion  to make a TiO2 film on silicon base?

One of the methods to deposite the TiO2 films is CVD.

But, can I sputter Ti on slilicon wafer first, and let the wafer w/ Ti
in high temperature

then the Ti will become TiO2?

I will appreciate your response.

Thank you.

Ralph Jih

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing