MEMSnet Home: MEMS-Talk: Hermetic sealing
Hermetic sealing
2001-10-05
Rong Hou
2001-10-09
[email protected]
2001-10-09
Erik Jung
Hermetic sealing
Erik Jung
2001-10-09
You can try VacSeal from SPI. This is a vacuum sealant - very useful
material!

SPI Supplies