Dear all,

I'm looking for SOI wafers with a handle thickness of 200 um (!), oxide
thickness of 2 um and a device thickness of 75 um. Especially the handle
thickness of only 200 um is quite demanding, but we can't do with thicker
handle layer. Does anybody know a supplier of such wafers?

Thanks a lot
Thomas

--------------------------------------------

Thomas Overstolz, PhD student
Institute of Microtechnology
University of Neuchbtel
Rue Jaquet-Droz 1
2007 Neuchbtel
Switzerland

Phone:   +41 (0)32 720 5619
Fax:     +41 (0)32 720 5711
mailto:  [email protected]
         http://www-samlab.unine.ch

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.