MEMSnet Home: MEMS-Talk: Quartz etched by HNO3?
Quartz etched by HNO3?
2001-10-17
Orjan Vallin
Quartz etched by HNO3?
Orjan Vallin
2001-10-17
I have experienced a roughening of the single crystalline quartz surface
when cleaning the sample in 800C concentrated nitric acid. Have you seen
the same thing, or have you some references to HNO3 crystalline quartz
cleaning?

Answers and hints on this subject would be most appreciated,

Orjan Vallin

reply