MEMSnet Home: MEMS-Talk: Adhesion
Adhesion
2001-11-08
madhulika sathe
Adhesion
madhulika sathe
2001-11-08
Hi,

I would like to find out how to address the improvement of adhesion between two
different types electroplated metals, to be specific Nickel,Iron and its
alloys.I would like to know a good reference material.

Thanks,
Madhulika Sathe
Research Assisstant
Mechanical Engineering Dept.
LSU

Phone : (225)578-4412
Fax   : (225)578-9195




Join 18 million Eudora users by signing up for a free Eudora Web-Mail account at
http://www.eudoramail.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing