MEMSnet Home: MEMS-Talk: Low Stress Nitride
Low Stress Nitride
2001-11-19
Roger Neef
2001-11-20
Roger Shile
2001-11-20
Kenneth Smith
Low Stress Nitride
Roger Shile
2001-11-20
JDS Uniphase in NC do low stress, low stress gradient SiN service.
The contact is:
Chris Sanders
(919)314-2258

>>> Roger Neef  11/19/01 03:17PM >>>
Hi,

Does anyone know where I can get service for the following.

Low stress PECVD nitride
2 um thick

Thank you for your help.

Regards,

Roger
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://fab.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Addison Engineering
The Branford Group