SiO2 and Pyrex Etching
2001-12-04
Paolo Bondavalli
2001-12-05
Roger Shile
SiO2 and Pyrex Etching
Paolo Bondavalli
2001-12-04
Dear MEMS experts,
I'm looking for details about the selectivity factor between the SiO2
and Pyrex when they are chemically etched.
Could you give me any references?
Thanks a lot

**********************************************
Dr. Paolo Bondavalli
R&D Engineer
LABCOM - Laboratoire Interconnexions Optiques et MEMS
THALES (ex THOMSON-CSF) CORPORATE RESEARCH CENTER
Domaine de Corbeville,
Route Departementale 128
F91404 ORSAY
(FRANCE)
Tel : 01 69 33 08 63
Fax : 01 69 33 08 62
Email : [email protected]
**********************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
University Wafer
Process Variations in Microsystems Manufacturing