Question for SU-8 photoresist adhesion problem.
2001-12-05
Tao Xu
2001-12-05
BERAUER,FRANK (HP-Singapore,ex7)
Question for SU-8 photoresist adhesion problem.
Tao Xu
2001-12-05
Hi,

    I met a question about SU-8 photoresist adhesion.
    I spun SU-8 on the SiO2/Si or Si3N4/Si substrate. After pattern the
SU-8, I put them into 30% KOH solution (80 degree C) to etch Si to form the
V-groove. However, SU-8 peeled off very quickly (just 1-2min) in the KOH
solution. The SU-8 is a part of my device and I want it to stay there after
KOH etching.
    Did anybody meet this problem and know how to solve it? Any suggestion
is high appreciation. Thanks in advance.

Regards,

Tao

_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
University Wafer