Hello Group,
Does anybody know if PZT precursor solutions are available commercially which I
can use for spin casting thin films straight from the bottle ? I am looking for
a stoichiometry of 52:48 ( Zr:Ti ).

Any possible leads will be much appreciated

Thanks in Advance.
--
K.Nandakumar.                           Tel : (216) 368 0397 (Off)
2549, KenilWorth Rd., #6,                     (216) 368 4109 (Lab)
Cleveland Heights, OH 44106.                  (216) 371 7786 (Res)


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.