MEMSnet Home: MEMS-Talk: KOH wet etching station
KOH wet etching station
2001-12-10
^Frank ^
2001-12-10
Mark West
2001-12-11
[email protected]
KOH wet etching station
^Frank ^
2001-12-10
Dear all,

I am wondering whether there is a kind of wet etching station that can
precisely control the bath temperature, the stirrer speed and rinse clean
the wafer?

Thanks,

frank

_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics