2001-12-31
Onnop Srivannavit
2001-12-31
wangzy-pim
etch Si(110) and Si(100) in KOH
Onnop Srivannavit
2001-12-31
Hi All

I etched Si(110) and Si(100) wafers in KOH using SiO2
as mask. I found that Si (110) surface after etch is
much rougher than Si(100) surface. I wonder if anyone
has experience about this. Does anyone know reasons
behind that?

Thanks in advance.

Onnop
Send your FREE holiday greetings online!
http://greetings.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Addison Engineering
Mentor Graphics Corporation