Hi,

Most photoresist with code beginning "AZ ..." is from Clariant

www.azresist.com
or
www.clariant.com


Laura

shaoning wrote:

> Hello, everybody,
>
> Does anyone know the contact info of manufacturer or vendor of AZ5214
> photoresist? It is said it can be reversed from positive to negative polarity
> by different baking. Thank you very much for every information.
>
> Shaoning
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

[demime 0.98e removed an attachment of type text/x-vcard which had a name of
laura.vcf]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review