MEMSnet Home: MEMS-Talk: Re: Metal sticking well to silicon and silicon nitride
Re: Metal sticking well to silicon and silicon nitride
1996-07-03
Mac McReynolds
1996-07-03
[email protected]
1996-07-04
Nutt Wolfgang
1996-07-04
Pierre Jaccard
1996-07-05
Padmaja Ramadas
1996-07-09
Bahram Ghodsian
1996-07-10
Mac McReynolds
1996-07-17
[email protected]
Re: Metal sticking well to silicon and silicon nitride
[email protected]
1996-07-03
Have you tried Al?