Electroplating Gold
Yohannes M Desta
2002-01-25
What type of solution (vendor and type) are you using? The vendor might have
an additive to improve the surface roughness.

Yohannes M Desta
CADM/LSU

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Sonia Garcia Blanco
Sent: Friday, January 25, 2002 9:23 AM
To: [email protected]
Subject: [mems-talk] Electroplating Gold


Dear All,

I am trying to electroplate gold on top of silica: for that I sputtered a
few nm Ti and then few nm of gold on top of the silica and place that in
the electroplating solution at 50C. I used a current of 50mA that will
give us around 2 micron thick layer of gold in 20min.

The surface appear with a lot of roughness.... Could somebody give me some
advice? Am I using the correct parameters for current and temperature to
get an uniform layer?

Thank you very much for your help!

Sonia.

*****************************************************

Sonia Garcia-Blanco

Department of Electronics and Electrical Engineering
University of Glasgow
Oakfield Ave.
G12 8LT
Glasgow

Phone:
   Office: (0141) 339 8855 ext 0101
   Lab:    (0141) 330 6014
Email: [email protected]

****************************************************
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
MEMStaff Inc.
Process Variations in Microsystems Manufacturing