Looking for platinum electrode for porous silicon formation
2002-01-29
Jin Zheng
Looking for platinum electrode for porous silicon formation
2002-01-29
Jeff Simkins
Looking for platinum electrode for porous silicon formation
Jeff Simkins
2002-01-29
try www.goodfellow.com for competitive prices and a wide range of sizes for
wires, rods, foils, plates, and maybe even mesh.

Jeff


-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Jin Zheng
Sent: Wednesday, January 30, 2002 1:33 AM
To: [email protected]
Subject: [mems-talk] Looking for platinum electrode for porous silicon
formation


Dear Mems Folks,

I am working on setting up a system for porous silicon formation. Can
anybody tell me where
I can find platinum plate or mesh for counter electrode. Thank you in
advance.

Best regards,

Jin Zheng
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation