Dear Pan,

Topsil Semiconductor Materials manufactures 6" high purity silicon by the
float zone technique. Please contact our sales department ([email protected],
Phone: +45 47365600) for further information.


Best regards,

Topsil Semiconductor Materials A/S

Jan Vedde
Quality- and project manager

Topsil Semiconductor Materials A/S
Linderupvej 4 ? P.O. Box 100
DK-3600 Frederikssund ? Denmark
Phone: +45 4736 5661 (direct)
Phone: +45 4736 5600 (switchboard)
Telefax: +45 4736 5601

-----Oprindelig meddelelse-----
Fra: Wanling Pan [mailto:[email protected]]
Sendt: 6. februar 2002 18:57
Til: [email protected]
Emne: [mems-talk] 6" high resitivity silicon wafer

Dear All,
  I am now trying to find some 6-inch high-resitivity silicon wafers, but
not of a huge amount. Maybe 5~20 of them would be enough for me. And I hope
the delivery could be quick enough. (I am in Belgium.) Could someone who has
information about this leave me a message (better if a price list is
accompanied)? Thanks a lot.

Best wishes,
  Wanling
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review