Inexpensive photomask service?
2002-02-06
Shan Jerry W CONT CRBE
2002-02-07
Blunier, Stefan
2002-02-08
Kun Lian
2002-02-08
Danny Hirdes
Inexpensive photomask service?
Danny Hirdes
2002-02-08
PageWorks (www.pageworks.com) can print transparencies with a resolution of
5080dpi.



-----Original Message-----
From: Shan Jerry W CONT CRBE 
Date: Wed, 6 Feb 2002 17:11:59 -0500
To: "'[email protected]'" 
Subject: [mems-talk] Inexpensive photomask service?


> I'm looking for a supplier that can inexpensively provide simple photomasks
within minimum feature size of 10 microns.  Is it possible to print the masks
from a postscript file?
>
> Any information would be highly appreciated.
>
> Thanks,
>
> Jerry
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
>
>

--

_______________________________________________
Win a ski trip!
http://www.nowcode.com/register.asp?affiliate=1net2phone3a

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics