MEMSnet Home: MEMS-Talk: Uniform nickel plating
Uniform nickel plating
2002-02-21
rtf
2002-02-21
Bigelow . Mike
Uniform nickel plating
Bigelow . Mike
2002-02-21
For high precision Ni and NiCo electroforming
please also visit our web site at www.drc.com

- Funnel shaped electroformed parts (apertures from 1 micron)
- Straight walled electroformed parts ( from 2 microns)
- Plating in support LIGA operations
- SU-8 parts

-Mike

_______________
Mike Bigelow
Technical Sales

DRC - Metrigraphics
60 Concord Street
Wilmington, MA 01887   USA

Tel:  + (978) 658-6100  ext. 3063
Fax: + (978) 657-7765


-----Original Message-----
From: rtf [mailto:[email protected]]
Sent: Thursday, February 21, 2002 11:50 AM
To: [email protected]
Subject: [mems-talk] Uniform nickel plating


Sou Zou,

There is a company in Syracuse NY (ReynoldsTech), that maybe able to
help you will nickel plating. They have   knowledge of nickel
deposition.

CN
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing