The mask of the Pt etch
2002-02-22
Hongjun Zeng
2002-02-25
Michael D Martin
The mask of the Pt etch
Hongjun Zeng
2002-02-22
Hello All,

Right now I'm trying to etch platinum. I checked in the THIN FILM PROCESSES
talking about the echant, it doesn't give a proper material for mask. Can
you please tell me by which mask material should I use in the Pt etching
process?

Thanks a lot,
Hongjun Zeng

Microfabrication Applications Laboratory (MAL)
University of Illinois at Chicago
ERF Building, 842 W. Taylor Street
Chicago, IL 60607-7022
Room 3014 ERF
Tel.: 312-413-5889, Fax: 312-996-6465

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review